PLA Filament Technical Specification                                                       

  • Filament Diameter: 1.75mm
  • Tolerance: ±0.05mm
  • Printing Temperature: 190°C-220°C
  • Heated Bed Temperature: 55-70°C
  • Printing Speed: 30-60mm/s

Highlights

High Gloss & Smoother: The surface of the silk PLA has some silky gloss so that print surface has less laminated striations and becomes smoother.

Higher Toughness: Silk PLA is close to standard PLA in material properties but it’s tougher than PLA.

High Quality: No bubble or dust inside filament, hardly clog the nozzle or extruder, designed to reduce jamming.                               

No Tangling: Perfect winded filament silk PLA, 100% tangle-free before unopened, neatly rolled, no curling or warping.  

High Compatibility: Universal compatibility with diverse 99% common-used FDM 3D printers in market.                                                                                         


Application and Target Audience

  • Beginners and DIY players.
  • Arts and crafts, 3D printing services.
  • Groups having high requirements about the surface expression of prints.


Relevant Parameters of Recommended Machine Types

Relevant Parameters of Recommended Machine Types

Type

Extruder Type/Heated Bed Type

Parameter

Creality Ender 3

Bowden/Flexible Bed Sticker

Printing Temperature: 200-220℃

Heated Bed Temperature: 55-65℃

Printing Speed: 30-60mm/s

Retracting Length: 2-4mm

Retracting Speed: 60-100mm/s

Creality CR-10

Bowden/Glass Bed

Printing Temperature: 200-220℃

Heated Bed Temperature: 65-70℃

 Printing Speed: 30-60mm/s

Retracting Length: 2-5mm

Retracting Speed: 80-110mm/s

 

 

Anycubic Mega-S

 

Bowden/ Microporous Coating Glass Bed

Printing Temperature: 200-220℃

Heated Bed Temperature: 60-70℃

Printing Speed: 30-60mm/s

Retracting Length: 2-4mm

Retracting Speed: 70-100mm/s

Prusa i3

Direct Drive Extruder/PEI Bed Sticker

Printing Temperature: 200-220℃

Heated Bed Temperature: 55-70℃

Printing Speed: 30-60mm/s

Retracting Length: 0.8mm

Retracting Speed: 30-40mm/s

Eryone Thinker S

Bowden/PEI Bed Sticker

Printing Temperature: 200-220℃

Heated Bed Temperature: 55-70℃

Printing Speed: 30-60mm/s

Retracting Length: 4mm

Retracting Speed: 90-110mm/s

Eryone Thinker SE

Bowden/Glass Bed

Printing Temperature: 200-220℃

Heated Bed Temperature: 65-70℃

Printing Speed: 30-60mm/s

Retracting Length: 4mm

Retracting Speed: 80-110mm/s

Eryone Thinker ER-20

Bowden/Silk-Screen Glass Bed

Printing Temperature: 200-220℃

Heated Bed Temperature: 60-70℃

Printing Speed: 30-60mm/s

Retracting Length: 2-5mm

Retracting Speed: 80-110mm/s

 

FAQ     

1.Q: Why my object printed with silk filament has no glossy surface?

A: You need to make sure that the printing temperature matches well with the printing speed. You need to adjust the printing temperature to 200-220℃.

2.Q: I failed to print small models with silk PLA. Why?

A: Silk PLA has silk texture, smooth surface and strong toughness, which is not suitable for printing high-precision or small-sized models.

3.Q: Why my filament tangles? How can I solve it?

A: The tangle of filament isn’t caused by the disordered or the imperfect winding. According to the production technology of filament, the filament winds back and forth (from left to right and then from right to left). Normally, there is no overline tangle. A common cause of tangle is that the filament end is not fixed to the holes of spool. Overline tangle or the changed winding direction make filament tangle. So customers need to fix the filament end to the proper holes of the spool.

4.Q: Can PLA be used to print tableware?

A: Not recommended. Although PLA is degradable, food-grade raw material, the PLA with toughener is non-food grade. If you really want to print a set of tableware, transparent PLA is suggested.

5.Q: The nozzle is clogged by PLA, and how can I solve it?

  A: Inconstant filament diameter, the lower nozzle temperature and frequent replacement with different kinds of filaments will lead to this problem. So, before you get started, clean the nozzle and turn up the temperature to a proper value.

6.Q: My prints have web-like strings (stringing) issues. How can I troubleshoot it?

  A: Too high temperature makes the PLA filament melt and flow so fast. Please turn the temperature down to a proper value.  

      The retracting parameters are improper, so adjust the retracting length and speed.  

7.Q: There are too much melted filament around the nozzle. What should I do?

  A: This problem can be attributed to over-high temperature, low printing speed, and in the slice software, the nozzle diameter doesn’t match with the extrusion output.

8.Q: The PLA filament was perfect when I opened the package. After several times of intermittent printing, my PLA filament snaps by accident during printing. Why?

A: Normally, the PLA filament in the printing process will not snap by themselves. However, after being affected by moisture, the degradable material PLA will be more brittle and easier to break, so you should pay attention to dampproof.

9.Q: The surface of my print isn’t very smooth. Why?

  A: The printing temperature is too high or too low. The temperature doesn’t match well with the printing speed. You need to adjust the printing speed or temperature.

10.Q: Why my PLA-printed objects don't stick to the heated bed? How do I solve?

A: The distance between the nozzle and the bed is too far. Make sure your heated bed is leveled and it’s clean. Then judge if the printing temperature and heated bed temperature are too low, and our customers should adjust them to correct ranges.

La base de conocimientos de Delivery&Return de Eryone3d

-Temporada de transporte y de entrega

-Como resultado de la venta de Eryone3d en múltiples regiones.por lo que la eficiencia del envío varía de región a región, de transportista a transportista. la siguiente información es sólo de referencia.

-Siga mi pedido primero.primero usted podría usar abajo el sitio web del transportista con el número de seguimiento que le enviamos

-Debido al impacto de la epidemia, la logística se verá afectada. Por favor, entienda y espere pacientemente.

Región

Portador

Tiempo de entrega (día)

Sitio web del transportista

Alemania

DHL

2-3

pista

Francia

DHL

4-6 pista

Otros UE countries(Italy,España etc)

DHL

4-6

pista

Otros países de la UE

GSL

4-6

pista

Otros países de la UE DPD 4-6 pista

REINO UNIDO

Correo Real

1-5

pista

US

Fedex

2-5

pista

US

UPS

2-7

pista

US

USPS

2-7

pista

CA

Fedex

1-5

pista

CA

Canadian Post

2-7

pista

CA

UPS

2-5

pista

Envío desde el almacén chino de Eryone (accesorios) 4PX 2-4 semanas pista
US,CA,EU,UK La logística de Amazon 1-7 días Contáctanos.

-Vuelva a

-Garantía: devolución sin condición dentro de 7 días para más, por favor lea la página de envío y devolución.

-Contacto

support@eryone.com

o en el chat en vivo con nosotros en el grupo de chat en vivo de Eryone.

domingo,lunes,martes,miércoles,jueves,viernes,sábado
enero,febrero,marzo,abril,mayo,junio,julio,agosto,septiembre,octubre,noviembre,diciembre
No hay suficientes ítems disponibles. Solo quedan [max].
Agregar a favoritosRevisar favoritosRemover favoritos
Bolsa de compras

Tu bolsa de compras está vacía.

Return To Shop

Agregar notas a la orden Editar notas de la orden
Estimar envío
Agregar un cupón

Estimar envío

Agregar un cupón

Tu código de cupón se aplicará en el checkout

Español

Select your language

USD

Selecciona tu moneda