Ender3/CR10/Mega-S/Thinker S/Thinker SE/ER-20 WITH BOWDEN EXTRUDER
Nozzle Temperature: 190~220℃
Heated Bed Temperature
1) PEI Magnetic Print Surface: 55~70℃
2) Glass Bed: 40°C-60°C
Print Speed: 10-30mm/s
Retract Length: 4~5mm
Ender3/CR10/Mega-S/Thinker S/Thinker SE/ER-20 WITH BOWDEN EXTRUDER
Nozzle Temperature: 190~220℃
Heated Bed Temperature
1) PEI Magnetic Print Surface: 55~70℃
2) Glass Bed: 40°C-60°C
Print Speed: 10-30mm/s
Retract Length: 4~5mm
ERYONE TPU gains popularity among 3D Printing community for its balance of rigidity and flexibility. In addition, with a 95A Shore Hardness and improved bed adhesion, it is easier to print even with a stock elementary 3D Printer like the Creality&Ender 3.From drone parts, phone cases, to small toys, all can be printed with ease.
ERYONE TPU filament 1.75mm is designed for hyper speed printing, 30-300mm/s up to 5 times faster than regular TPU filament, providing a smooth and efficient 3D printing experience.
Make it easy to print, faster than previous TPU, excellent adhesion. Clog-Free, Bubble-Free, Low-Warp, Low-String.
is a polymer material between rubber and plastic. It has excellent high tension, high tensile strength, toughness and aging resistance. It is a mature environmental protection material. TPU consumables are added on the basis of raw materials. The material is environmentally friendly.
Print Temperature:190 - 220℃, Diameter:1.75mm (Tolerance:+/-0.05mm). Shore hardness 95A, Net weight 1kg2.2lbs), We recommend hardened steel nozzle 0.5mm.
Yes. The material itself is soft and does not bear any force. It is recommended to use the direct drive extruder to get a good printing experience. The remote extruder can only print normally after modification.
No, you don't have to. You can print objects normally when the heated bed is at room temperature.
The tangle of filament isn’t caused by the disordered or the imperfect winding. According to the production technology of filament, the filament winds back and forth (from left to right and then from right to left). Normally, there is no overline tangle. A common cause of tangle is that the filament end is not fixed to the holes of spool. Overline tangle or the changed winding direction make filament tangle. So customers need to fix the filament end to the proper holes of the spool.
Inconstant filament diameter, the lower nozzle temperature and frequent replacement with different kinds of filaments will lead to this problem. So, before you get started, clean the nozzle and turn up the temperature to a proper value.
Too high temperature makes the TPU filament melt and flow so fast. Please turn the temperature down to a proper value.
The retracting parameters are improper, so adjust the retracting length and speed.
This problem can be attributed to over-high temperature, low printing speed, and in the slice software, the nozzle diameter doesn’t match with the extrusion output.
The printing temperature is too high or too low. The temperature doesn’t match well with the printing speed. You need to adjust the printing speed or temperature.