PLA + (PLA più resistente, facile da usare)

$29.94

Shipping calculated at checkout.

· codice 10% ERYONE3D al momento del pagamento, SCONTO DEL 15% sull'acquisto di 6 o più rotoli & nbsp;


· Recensito da John Aldred & nbsp;
<⇨Eryone PLA + filamento per stampante 3D. È migliore del PETG?
· Recensione di Andrew Sink & nbsp; & nbsp;

Stampa 3D con filamento REALLY WET / Eryone PLA +

· Più resistente del PLA standard.
· Diametro del filamento accurato (mm) 1,75 ± 0,03 , Estrusione uniforme sotto i 200 ℃.
·· Adattamento ad ampia temperatura, stampa molto buona tra 190-230 ℃ senza ostruzioni.
·· Puoi ottenere le stampe più straordinarie, lucide, lisce e belle tra 200-220 ℃.
· Funziona molto bene con le tue stampanti ..
· Peso netto 1 kg, Peso di spedizione 1,28 kg & nbsp ;.
· Temperatura di stampa consigliata (℃) 200 ~ 230.
·· Velocità di stampa consigliata (mm / s) 30 ~ 70.
· Consiglia letto riscaldato (℃) 60 ~ 70

preorder ends in

dayshoursminssecs

Testimonial

·MAKERS'REVIEW

PLA PLUS, ROBUSTEZZA PLUS

Rispetto al PLA standard, il PLA + ha migliorato lo svantaggio della tenacità del PLA non buona. La qualità delle parti stampate è ancora molto buona e la stessa del PLA standard.

Perché è speciale

Buona adattabilità alla temperatura, può ottenere buoni risultati di stampa nell'intervallo di 200 ~ 230 ℃

Più adatto per i principianti

Buona fluidità, compatibile con la maggior parte delle stampanti 3D FDM sul mercato

La superficie di stampa è liscia e l'effetto è buono

Più resistente del PLA, migliori prestazioni di resistenza alla trazione

Specifica

Spec.

Valore

Diametro del filamento (mm)

1.75±0.03

N.W (kg)

1

Peso specifico (g / cm3)

1.24

Consiglia temperatura di stampa (℃)

200~230

Consiglia velocità di stampa (mm / s)

30~70

Consiglia letto riscaldato (℃)

60~70

Temperatura di deflessione del calore (0,45 MPa) (℃)

60

Assorbimento dell'umidità

Cattivo

Consiglia la temperatura di conservazione (℃)

0~32


Domande frequenti

Se il filamento non viene utilizzato per un lungo periodo, tenerlo in un ambiente fresco (temperatura inferiore a 32 ℃) e asciutto (umidità inferiore al 40%) per tempo.

Utilizzare un panno morbido per pulire gli ugelli prima e dopo la stampa per evitare che il filamento residuo influenzi la stampante

Se c'è un problema di intasamento, controllare se la molla di alimentazione è troppo allentata e fa sì che il consumabile slitti / troppo stretto, il che causa il danneggiamento del filamento dall'ingranaggio;


The test results are as follows:

①The diameter of the PLA+ is within the allowable error range, and the filament is evenly extruded esat 200℃;

②Good temperature characteristics, smooth extrusion at 190-230℃, no jamming, work well
③The most suitable temperature for PLA+ is 200-220℃. within the range, the filament extrusion is continuous and smooth, the gloss is high, the printing surface is smooth, and the color is beautiful; (the temperature on the label is 200-230℃)
④ PLA+ have good compatibility and are suitable for use on most printers on the market;
⑤Compared with Standard PLA, the proportion of toughening agent is increased, the toughness is better, and it is not easy to break. There is no fracture in the test process;
⑥ Good adhesion ;
⑦It is emphasized that PLA+ have a characteristic, the printing temperature and printing speed must be matched, so that the desired effect can be produced. In addition, the matching degree of retraction is also high, which can reduce stringing. In summary, the test passed.
Recommended printing temperature: 200-220℃; Recommended printing speed: 30-70mm/s; Recommended hot bed temperature: 60-70℃; Recommended withdrawal: length: 6mm, speed: 110mm/s; (remote printer) length: 0.8mm, speed: 35-40mm/s; (short-range printer) Applicable models: mainstream Ender-3/CR-10/Prusa i3/thinker S/thinker SE/ER-20, etc.

FAQs
If the filament is not used for a long time, please keep them in a cool (temperature lower than 32℃) and dry environment (humidity lower than 40%) in time.
Please use a soft cloth to clean the nozzles before and after printing to prevent the residual filament from affecting the printer
If there is a problem of the clog, please check whether the feeder spring is too loose and causes the consumable to slip/too tight, which causes the filament to be damaged by the gear.
Sunday,Monday,Tuesday,Wednesday,Thursday,Friday,Saturday
January,February,March,April,May,June,July,August,September,October,November,December
Not enough items available. Only [max] left.
Shopping cart
Free Shipping for all orders over [money]
Almost there, add [money] more to get FREE SHIPPING!
Congratulations! You've got free shipping!

Your cart is empty.

Return To Shop

Add Order NoteEdit Order Note
Add A Coupon

Add A Coupon

Coupon code will work on checkout page

PLA + (PLA più resistente, facile da usare)

EU / Green / 9% : ERYONE3D 11% : signup to get 14%: Buy 10 rolls12%-15% : get from affiliate
EU / Green / 9% : ERYONE3D 11% : signup to get 14%: Buy 10 rolls12%-15% : get from affiliate
$29.94